MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® K225-KV PA6 FR(30), Dry, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Unreinforced, Flame Retardant

Material Notes: Flame Retardant (halogen free), Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 7.5 %7.5 %Sim. ISO 62
Moisture Absorption 2.00 %2.00 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa10200 psiISO 527-1/-2
Elongation at Break 4.0 %4.0 %Nominal; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %ISO 527-1/-2
Tensile Modulus 4.20 GPa609 ksiISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60250
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Dissipation Factor  0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Flammability, UL94  V-2
@Thickness 0.380 mm
V-2
@Thickness 0.0150 in
IEC 60695-11-10
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
IEC 60695-11-10
Glow Wire Ignition Temperature  850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
 930 °C
@Thickness 0.380 mm
1710 °F
@Thickness 0.0150 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.380 mm
1760 °F
@Thickness 0.0150 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSM8061 / 184762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.