MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 8502-5/AboCure 8502-5 Colorless, Low-Exotherm Epoxy Casting Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8502-5/AboCure 8502-5 is a rigid, colorless, low-exotherm epoxy casting compound for spherical masses up to 500 grams. It is a 2-component structural and dielectric liquid system with extremely low shrinkage. The size of its castings is limited by its exotherm (heat of reaction) in bulky casings. In such cases, casting is done in successive thinner layers (to avoid excessive exotherm) until the desired thickness is reached. It gives superior decorative and laboratory embedments and table- and counter-top castings for restaurants and bars. Lower cost versions are known as "decoupage" resins. Many faster-curing versions are also available. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens for commercial or scientific uses. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 1.1 %
@Time 28800 sec
1.1 %
@Time 8.00 hour
boil
Viscosity 400 cP400 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585
Tensile Strength, Ultimate 67.78 MPa9831 psi
Flexural Strength 103.05 MPa14946 psi
Flexural Modulus 3.52 GPa510 ksi
Compressive Strength 99.547 MPa14438 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 - 80.0 °C140 - 176 °FDeflection Temp at unknown load
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
2nd step
 60.0 - 360 min
@Temperature 80.0 - 110 °C
1.00 - 6.00 hour
@Temperature 176 - 230 °F
optional 3rd step
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
1st step
Pot Life 300 - 360 min300 - 360 min
 
Descriptive Properties
Acetone Absorption (%)8.83 hr. boil
ColorClear
Parts by Weight (pbw)100AboCast
 30AboCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCast 8504-5 One-Component Epoxy
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy
Abatron AboCast 50-3/AboCure 50-12 Epoxy
Abatron AboCast 50-11/AboCure 50-12 Epoxy

PABC894 / 107878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.