MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin NEOFLON M-300PL PCTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: NEOFLON PCTFE M-300PL is a high hardness fluororesin with excellent gas barrier properties.

Introduction: NEOFLON PCTFE M-300PL is a polymer with a structure in which all hydrogen atoms of polyvinyl chloride (CH2 --CHCl) n are substituted with fluorine atoms. It is in the form of one chlorine atom in PTFE structural unit; Highly transparent due to this chlorine atom; It is a fluororesin with the highest gas barrier property and high hardness; Excellent in mechanical properties, although it is slightly inferior to PFA and FEP in heat resistance and chemical resistance; M-300PL is a pelletized product with higher molecular weight than M-300P; Excellent in stress crack resistance. It is suitable for both compression and extrusion molding

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.13 g/cc2.13 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.080.0ASTM D 638
Tensile Strength 44.7 MPa6480 psiASTM D1708
Elongation at Break 163 %163 %ASTM D1708
 
Thermal PropertiesMetricEnglishComments
Melting Point 212 °C414 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIK9698 / 327138

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.