MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi PET-G 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: PET-G is a strong, high clarity, odor neutral and easy to print filament for 3D printing. These characteristics, together with the high impact strength, excellent flexibility, and practically no shrinkage make PET-G an excellent material that combines the advantages of both PLA and ABS. In short, PET-G has many great features and is the perfect addition to any filament assortment.

Features:

  • High clarity
  • Strong & Flexible
  • Almost no “warping”
  • Odor neutral printing
Colors: PET-G is available from stock in 19 colors. Other colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccISO 1183
Filament Diameter 1750 µm1750 µmTolerance: 50 µm, =95% Roundness
 2850 µm2850 µmTolerance: 100 µm, =95% Roundness
Melt Flow 6.4 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.4 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiISO 527
Elongation at Break 23 %23 %ISO 527
Elongation at Yield 6.0 %6.0 %ISO 527
Tensile Modulus 2.02 GPa293 ksi(E); ISO 527
Flexural Strength 69.0 MPa10000 psiISO 178
Flexural Modulus 2.05 GPa297 ksiISO 178
Charpy Impact, Notched 0.810 J/cm²3.85 ft-lb/in²ISO 179 1eA
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °FHeat Deflection Temperature; ISO 75
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 250 °C446 - 482 °FPrinting Temperature
 
Descriptive Properties
Bed Temp=70°C
Moisture Absorption1104 ppmISO 62
Rockwell Hardness105ASTM D785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9834 / 301059

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.