MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shakespeare Isocor™ HG20SC Nylon 612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Carbon Fiber Filled; Nylon 612 (PA612)

Material Notes: Isocor™ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability. Isocor™ HG20SC is used in applications requiring good electrical insulation properties. This resin can be processed with conventional techniques.

Used for injection molding, automotive, lawn and garden, tubing, and films.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.039 g/cc0.03754 lb/in³ASTM D 792
Moisture Absorption 0.17 %0.17 %ASTM D 570-95
Linear Mold Shrinkage 0.012 cm/cm
@Thickness 3.17 mm
0.012 in/in
@Thickness 0.125 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 31.4 MPa4560 psiASTM D 638
Tensile Modulus 2.30 GPa333 ksiASTM D 638
Izod Impact, Notched 0.366 J/cm0.685 ft-lb/inASTM D 256
Gardner Impact 36.2 J
@Temperature 23.0 °C
26.7 ft-lb
@Temperature 73.4 °F
ASTM 5420
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FASTM D 3418-97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSC-10/4 EC black 9832 PA666-CF
Shakespeare Isocor™ HG26SI medium viscosity PA-612
Shakespeare Isocor™ TT52SI Nylon 6 Terpolymer
DSM Fibre Intermediates Nyrim® 3000 (Dry)
DSM Fibre Intermediates Nyrim® 1500 (Conditioned)

PSHAKE118 / 67397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.