System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel
ATI Allegheny Ludlum 410 Martensitic Stainless Steel
ATI Allegheny Ludlum 420 Martensitic Stainless Steel
ATI Allegheny Ludlum 420ESR Tool Steel, UNS S42000
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
ATI Allegheny Ludlum 430 Ti Controlled Expansion Alloy, UNS K91800
ATI Allegheny Ludlum 440A Martensitic Stainless Steel
ATI Allegheny Ludlum 441HP™ Stainless Steel Alloy
ATI Allegheny Ludlum A2 Tool Steel, UNS T30102
ATI Allegheny Ludlum A6 Tool Steel, UNS T30106
ATI Allegheny Ludlum A7 Tool Steel, UNS T30107
ATI Allegheny Ludlum AL 13-8™ H 1000 Precipitation Hardening Alloy
ATI Allegheny Ludlum AL 13-8™ H 1025 Precipitation Hardening Alloy
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F
ATI Allegheny Ludlum AL 13-8™ H 1100 Precipitation Hardening Alloy
ATI Allegheny Ludlum AL 13-8™ H 950 Precipitation Hardening Alloy
ATI Allegheny Ludlum AL 15-5 High Strength Stainless Steel, UNS S15500
ATI Allegheny Ludlum AL 15-7 High Strength Stainless Steel, UNS S15700
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400
ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200
ATI Allegheny Ludlum AL 201™ Nickel Alloy, UNS N02201
ATI Allegheny Ludlum AL 20™ Plate Specialty Steel
ATI Allegheny Ludlum AL 20™ Sheet and Strip Specialty Steel
ATI Allegheny Ludlum AL 219 High Strength Specialty Steel Alloy (Alloy 21-6-9), UNS S21904
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Plate > 0.1875" Duplex Stainless Steel, UNS S31803
ATI Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Sheet and Strip < 0.1875", UNS S31803
ATI Allegheny Ludlum AL 22-3 Controlled Expansion Alloy
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
ATI Allegheny Ludlum AL 29-4® Superferritic Stainless Steel, UNS S44700
ATI Allegheny Ludlum AL 29-4-2® Duplex Stainless Steel, UNS S44800
ATI Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Annealed Plate, Sheet, and Strip, UNS N04400
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Heavily Cold Rolled Sheet and Strip, UNS N04400
ATI Allegheny Ludlum AL 400™ Nickel-Base Alloy, Hot Rolled Plate, UNS N04400
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 16.4% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 2.9% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 20% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 34.5% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930
ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr
ATI Allegheny Ludlum AL 418™ Special (Greek Ascoloy) Martensitic Stainless Steel
ATI Allegheny Ludlum AL 42™ Electrical Alloy, UNS K94100
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
ATI Allegheny Ludlum AL 440C™ Martensitic Stainless Steel, UNS S44004
ATI Allegheny Ludlum AL 444™ Ferritic Stainless Steel
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel
ATI Allegheny Ludlum AL 453™ Stainless Steel
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel
ATI Allegheny Ludlum AL 45™ Magnetic Alloy
ATI Allegheny Ludlum AL 468™ Dual Stabilized- Low Titanium Stainless Steel
ATI Allegheny Ludlum AL 4750™ Electrical Alloy, UNS K94800 or UNS K95000
ATI Allegheny Ludlum AL 50™ High Strength Stainless Steel, UNS S20910
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, 1149°C (2100°F) Solution Treated, UNS N06601
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601
ATI Allegheny Ludlum AL 610 Stainless Steel, UNS S30600
ATI Allegheny Ludlum AL 611 Stainless Steel, UNS S30601
ATI Allegheny Ludlum AL 625HP™ Stainless Steel
ATI Allegheny Ludlum AL 800AT™ Nickel-Base Alloy, UNS N08811
ATI Allegheny Ludlum AL 800H™ Nickel-Base Alloy, UNS N08810
ATI Allegheny Ludlum AL 800™ Nickel-Base Alloy, UNS N08800
ATI Allegheny Ludlum AL 825™ Nickel Alloy
ATI Allegheny Ludlum AL Altemp® 625 Nickel-Base Superalloy, UNS N06625
ATI Allegheny Ludlum AL-6XN PLUS™ Superaustenitic Stainless Steel
ATI Allegheny Ludlum ALFA-II™ Stainless Steel Type 406
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
ATI Allegheny Ludlum ALFA-IV™ Oxidation Resistant Alloy
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy
ATI Allegheny Ludlum Alloy 255 Duplex Stainless Steel, UNS S32550
ATI Allegheny Ludlum Alloy G3 Corrosion Resistant Alloy, UNS N06985
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Sheet and Strip, UNS N07718
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
ATI Allegheny Ludlum Altemp® X-750 Nickel-Based superalloy
ATI Allegheny Ludlum AM 350™ High Strength Specialty Steel Alloy, Condition DA, Sheet and Strip, UNS S35000
ATI Allegheny Ludlum AM 355™ High Strength Alloy, UNS S35500
ATI Allegheny Ludlum ATI 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
ATI Allegheny Ludlum D2 Tool Steel, UNS T30402
ATI Allegheny Ludlum E-BRITE 26-1® Superferritic Stainless Steel, UNS S44627
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250)
ATI Allegheny Ludlum Grade 11 Titanium (UNS R52250)
ATI Allegheny Ludlum Grade 12 Titanium (UNS R53400)
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402)
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252)
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322)
ATI Allegheny Ludlum Grade 2 Titanium (UNS R50400)
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550)
ATI Allegheny Ludlum Grade 4 Titanium (UNS R50700)
ATI Allegheny Ludlum Grade 5 Titanium 6Al-4V (UNS R56400)
ATI Allegheny Ludlum Grade 7 Titanium (UNS R52400)
ATI Allegheny Ludlum Grade 9 Titanium (UNS R56320, Ti 3Al-2.5V)
ATI Allegheny Ludlum H13 Tool Steel, UNS T20813
ATI Allegheny Ludlum K12® Dual Hardness Steel
ATI Allegheny Ludlum M2 Tool Steel, UNS T11302
ATI Allegheny Ludlum M3 Tool Steel, UNS T11313
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Annealed
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 288°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 316°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 427°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 482°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 649°C (1200°F) Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Annealed
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 316°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 427°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Annealed
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 288°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 316°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 427°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 482°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 538°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 649°C (1200°F) Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Annealed
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 204°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 316°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 427°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 482°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 538°C Temper
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 649°C (1200°F) Temper
ATI Allegheny Ludlum MINIMISER® 304/304L Stainless Steel
ATI Allegheny Ludlum MINIMISER® 316/316L Stainless Steel
ATI Allegheny Ludlum Moly Permalloy Electrical Alloy
ATI Allegheny Ludlum Ohmaloy® 30 Resistance Alloy
ATI Allegheny Ludlum Relay Steels No. 2
ATI Allegheny Ludlum Relay Steels No. 5
ATI Allegheny Ludlum S7 Tool Steel, UNS T41907
ATI Allegheny Ludlum Sealmet® 4 Controlled Expansion Alloy, UNS K94760
ATI Allegheny Ludlum Sealmet® 485 Controlled Expansion Alloy
ATI Allegheny Ludlum Silectron® Electrical Steel- Grain Oriented Type
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400)
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008)
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904)
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367)
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 20% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 30% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 40% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 50% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 60% Cold Work
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 0% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 10% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 30% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 50% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 20% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, Annealed (UNS S30400)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 10% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 30% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 50% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 0% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 50% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 60% Cold Rolled (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-6 (UNS S20153)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-7 (UNS S20153)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-8 (UNS S20153)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726)
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 303, Annealed (UNS S30300)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 538°C (UNS S41600)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 593°C (UNS S41600)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 649°C (1200°F) (UNS S41600)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600)
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 760°C (UNS S41600)
ATI Allegheny Ludlum Stainless Steel JS700® Alloy (UNS N08700)
ATI Allegheny Ludlum Stainless Steel Ohmaloy® 40 Resistance Alloy
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 30% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 40% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 50% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 20% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 30% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 5% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 50% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 201L, Annealed (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, 1/4 Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100)
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700)
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800)
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 50% cold work (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 70% cold work (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum T-436 Ferritic Stainless Steel, UNS S43600
ATI Allegheny Ludlum Type 310L Stainless Steel
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700
ATI Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.