S-Glass Fiber, Generic
Most of the data in MatWeb has been supplied directly by companies in the supply chain -
the manufacturers, or, less commonly, distributors or fabricators. Other data
has been provided by standards organizations or from similar materials/known relationships by
the MatWeb staff. For more information about this specific material, see the following source(s):
Advanced Thermoset Composites - Industrial and Commercial Applications, James M. Margolis, Van Nostrand Reinhold Co., NY, (1986)
Analysis and Performance of Fiber Composites, 2nd ed., Bhagwan D. Agarwal and Lawrence J. Broutman, John Wiley & Sons, Inc., NY, (1990)
ASM Engineered Materials Reference Book, Second Edition, Michael Bauccio, Ed. ASM International, Materials Park, OH, 1994.
Carbon Fiber Composites, Deborah D. L. Chung, Butterworth-Heinemann, Boston, MA, (1994)
Handbook of Biomaterial Properties, Jonathan Black, Garth Hastings, Ed., Chapman & Hall: London; New York, 1998