MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: (PC+PBT)-blend, impact modified, Injection molding grade, high toughness at low temperatures, ideal for painted applications, unreinforced

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.50 %0.50 %ISO 62
Viscosity 670 cP
@Frequency 165 Hz,
Temperature 260 °C
670 cP
@Frequency 165 Hz,
Temperature 500 °F
Gottfert melt
Melt Flow 19 g/10 min
@Load 5.00 kg,
Temperature 260 °C
19 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 100 MPa14500 psiISO 2039-1
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1/-2
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.15 GPa312 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 75.0 MPa10900 psi2 mm/min; ISO 178
Flexural Yield Strength 66.0 MPa
@Strain 3.5 %
9570 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa305 ksi2 mm/min; ISO 178
Flexural Strain at Yield 5.5 %5.5 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  45.0 kJ/m²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 52.0 kJ/m²
@Temperature -20.0 °C
24.7 ft-lb/in²
@Temperature -4.00 °F
ISO 180-A
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180-U
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 6.00 J/cm²28.6 ft-lb/in²ISO 179/1eA
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0015
@Frequency 100 Hz
0.0015
@Frequency 100 Hz
IEC 60250
 0.013
@Frequency 1e+6 Hz
0.013
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 V100 VCTI M; Solution B; IEC 60112
 500 V500 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Thermal Conductivity 0.179 W/m-K1.24 BTU-in/hr-ft²-°F
Melting Point 223 °C433 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 106 °C223 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FISO 75-1/-2
Vicat Softening Point 125 °C
@Load 5.10 kg
257 °F
@Load 11.2 lb
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
Oxygen Index 21 %21 %Method A; ISO 4589-1/-2
Glow Wire Flammability Index 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 70.0 °C158 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade
Covestro Makroblend® UT5205 PC/PBT Blend
Barlog Plastics KEBATER A1100 PBT/PC unreinforced, high impact
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized

PB09852 / 92692

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.