MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Garlock 509 Butyl Sheet Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Style #509 is a branded, chloro-butyl sheet rubber product.

Information provided by Garlock Rubber Technologies

Key Words: IIR isobutylene isoprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Oil Absorption 10 %
@Temperature 150 °C,
Time 252000 sec
10 %
@Temperature 302 °F,
Time 70.0 hour
Oil Immersion Test No. 3; ASTM D471
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6555 - 65
 70 - 80
@Treatment Temp. 125 °C,
Time 252000 sec
70 - 80
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged
Tensile Strength >= 10.3 MPa>= 1500 psi
 12.4 MPa1800 psiTypical
Elongation at Break >= 350 %>= 350 %
 >= 300 %
@Treatment Temp. 125 °C,
Time 252000 sec
>= 300 %
@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set 60 %
@Temperature 100 °C,
Time 79200 sec
60 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -34.4 °C-30.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sibur BK-1675M Butyl Rubber (IIR)
ATG s.r.l. IIR Butyl Rubber
Butyl Rubber (IIR, CIIR, BIIR)
Trelleborg T528 Butyl Rubber
Sibur BK-1675N Butyl Rubber (IIR)

PGARL990 / 157463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.