MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Magnesium AZ81A-T4, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Sand Castings: ASTM B 80. Permanent Mold Castings: ASTM B 199. Investment Castings: B403. Readily castable, has a low microshrinkage tendency, and is used in the solution-treated condition (T4 temper). Typically used for commercial and military permanent-mold and investment castings requiring good strength and excellent ductility and toughness. Good castability tough, pressure tight.

Key Words: UNS M11810; Electron A8; Mg; ASTM B 80; ASTM B 199; ASTM B 403; SAE J465; Old SAE 505; European EN 1753 MC21110 (Ingot UNS M11811)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5555500 kg load, 10 mm ball
Hardness, Knoop 7070Estimated from Brinell
Hardness, Rockwell E 6666
Tensile Strength, Ultimate 275 MPa39900 psi
Tensile Strength, Yield 83.0 MPa
@Strain 0.2 %
12000 psi
@Strain 0.2 %
Elongation at Break 15 %15 %in 50 mm
Tensile Modulus 45.0 GPa6530 ksi
Compressive Yield Strength 83.0 MPa12000 psiat 0.2% offset
Ultimate Bearing Strength 400 MPa58000 psi
Bearing Yield Strength 240 MPa34800 psi
Poissons Ratio 0.340.34
Fatigue Strength 76.0 MPa
@# of Cycles 1.00e+8
11000 psi
@# of Cycles 1.00e+8
R.R. Moore Test
Machinability 100 %100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa2470 ksi
Shear Strength 125 MPa18100 psi
Charpy Impact 6.10 J4.50 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000150 ohm-cm0.0000150 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 370 J/g159 BTU/lb
CTE, linear  25.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.9 µin/in-°F
@Temperature 32.0 - 212 °F
 27.2 µm/m-°C
@Temperature 20.0 - 200 °C
15.1 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Thermal Conductivity 51.1 W/m-K355 BTU-in/hr-ft²-°F
Melting Point >= 421 °C>= 790 °FIncipient Melting
Solidus 490 °C914 °F
Liquidus 610 °C1130 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 705 - 845 °C1300 - 1550 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 7.0 - 8.1 %7.0 - 8.1 %
Copper, Cu <= 0.10 %<= 0.10 %
Magnesium, Mg 92 %92 %As Remainder
Manganese, Mn >= 0.13 %>= 0.13 %
Nickel, Ni <= 0.010 %<= 0.010 %
Silicon, Si <= 0.30 %<= 0.30 %
Zinc, Zn 0.40 - 1.0 %0.40 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AZ80A-T5, Extruded
Aluminum 7075-T6; 7075-T651
Magnesium AZ80A-F, Forged
Magnesium AZ80A-T5, Forged
Alclad Aluminum 7075-T6, T651

MMAZ84 / 12332

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.