MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem RP 141 Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent processability.

Applications: Cosmetic packaging; containers for freezer; disposable packages with high transparency.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792A
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8383ASTM D785
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Elongation at Yield 14 %14 %ASTM D638
Flexural Modulus, 1% Secant 1050 MPa152000 psiASTM D790
Izod Impact, Notched  0.200 J/cm
@Temperature -20.0 °C
0.375 ft-lb/in
@Temperature -4.00 °F
ASTM D256A
 0.400 J/cm
@Temperature 23.0 °C
0.749 ft-lb/in
@Temperature 73.4 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C181 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C120 °FASTM D648
Vicat Softening Point 127 °C261 °F10 N; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 18 %18 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem PRA 0852 RACO Random Polypropylene Copolymer
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Braskem CP 401 HC Injection Molding Polypropylene
Braskem CP 442 XP Injection Molding Polypropylene
Braskem PRB 0131 RACO Random Polypropylene Copolymer

PBRAS028 / 27762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.