MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Edinburg Plastics AGG645 ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Appearance: Opaque- Black, Gray

Processing Methods: Injection

Applications: Automotive, Appliance, AC Fan

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792-91
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D955
Melt Flow 4.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 68.9 MPa10000 psiASTM D638
Flexural Yield Strength 86.2 MPa12500 psiASTM D790
Flexural Modulus 5.03 GPa730 ksiASTM D790
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 187 - 204 °C369 - 399 °F
Middle Barrel Temperature 204 - 232 °C399 - 450 °F
Front Barrel Temperature 218 - 246 °C424 - 475 °F
Nozzle Temperature 218 - 274 °C424 - 525 °F
Melt Temperature 218 - 274 °C424 - 525 °F
Mold Temperature 63.0 - 85.0 °C145 - 185 °F
Injection Velocity 25.4 - 127 mm/sec1.00 - 5.00 in/sec
Drying Temperature 82.0 - 93.0 °C180 - 199 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Dew Point >= -26.1 °C>= -15.0 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiLower is better
Vent Depth 0.00381 - 0.00508 cm0.00150 - 0.00200 in
Screw Speed 20 - 60 rpm20 - 60 rpmLower is better
 
Descriptive Properties
AppearanceOpaque-Black and Gray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Edinburg Plastics AGG625 ABS
Birch Plastics RPP1215 Recycled Polypropylene
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade

PEDIN004 / 183507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.