MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arlon Electronic Materials 33N Polyimide Laminate and Prepreg
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: High reliability and high temperature material

33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with flame retardance. High Tg results in low overall processing and minimizes risk of latent PTH defects in-service.

  • Low Z-expansion minimizes the risk of PTH defects caused during solder reflow and device attachment
  • Electrical and mechanical properties meeting the requirements of IPC-4101/40 and /41
  • Toughened. Non-MDA chemistry resists drill cracking
  • Compatible with lead-free processing
  • RoHS/WEEE compliant

Typical Applications:

  • PCBs that are subjected to high temperatures during processing, such as lead-free soldering
  • Applications with significant lifetimes at high temperatures, such as aircraft engine instrumentation, down hole drilling, under-hood automotive controls, burn-in boards, or industrial sensors.

Information provided by ARLON Electronic Materials.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM D792 Method A
Water Absorption 0.21 %0.21 %IPC TM-650 2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 22.1 GPa3200 ksiIPC TM-650 2.4.18.3
Poissons Ratio 0.150.15ASTM D3039
Peel Strength 1.26 kN/m7.20 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 1.26 kN/m7.20 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 1.31 kN/m7.50 pliTo Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.20e+13 ohm-cm7.20e+13 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
 4.50e+14 ohm-cm4.50e+14 ohm-cmE24/125; IPC TM-650 2.5.17.1
Surface Resistance 4.10e+14 ohm4.10e+14 ohmC96/35/90; IPC TM-650 2.5.17.1
 1.60e+15 ohm1.60e+15 ohmE24/125; IPC TM-650 2.5.17.1
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
Dielectric Strength 50.8 kV/mm1290 kV/inIPC TM-650 2.5.6.2
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
Arc Resistance 170 sec170 secIPC TM-650 2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 - 17.0 µm/m-°C8.89 - 9.44 µin/in-°FIPC TM-650 2.4.41
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature <=250 °C
30.6 µin/in-°F
@Temperature <=482 °F
z (< Tg); IPC TM-650 2.4.24
 164 µm/m-°C
@Temperature >=250 °C
91.1 µin/in-°F
@Temperature >=482 °F
z (> Tg); IPC TM-650 2.4.24
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM E1461
Glass Transition Temp, Tg 250 °C482 °FTMA; IPC TM-650 2.4.24
Decomposition Temperature 353 °C667 °FOnset; IPC TM-650 2.4.24.6
 389 °C732 °F5 percent; IPC TM-650 2.4.24.6
Flammability, UL94 V-0V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)23IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)8IPC TM-650 2.4.24.1
Z-Axis Expansion (%)1.2IPC TM-650 2.4.24 (50-260°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arlon Electronic Materials 85N Polyimide Laminate and Prepreg
Arlon Electronic Materials 35N Fast Cure Polyimide Laminate and Prepreg
Arlon Electronic Materials EP2 Enhanced Polyimide Laminate and Prepreg
Oxygen-free electronic Copper, UNS C10100
Rogers Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards

PARLM9861 / 149014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.