MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exxtral™ BMU 130 Performance Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.

Availability: Europe

Features:

  • Balanced Stiffness/Toughness
  • Ductile
  • Good UV Resistance
  • Good Weather Resistance
  • High Impact Resistance
  • Low Temperature Impact Resistance
Uses:
  • Automotive Bumper
  • Automotive Exterior Parts
  • Automotive Trim
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 11.6 MPa1680 psiISO 527-2
Tensile Strength, Yield 15.1 MPa2190 psiISO 527-2
Elongation at Break 79 %79 %ISO 527-2
Elongation at Yield 4.3 %4.3 %ISO 527-2
Tensile Modulus 1.20 GPa174 ksiSecant; ISO 527-2
Charpy Impact, Notched  0.798 J/cm²
@Temperature -30.0 °C
3.80 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179
 1.09 J/cm²
@Temperature -20.0 °C
5.20 ft-lb/in²
@Temperature -4.00 °F
Complete Break; ISO 179
 6.51 J/cm²
@Temperature 22.8 °C
31.0 ft-lb/in²
@Temperature 73.0 °F
Partial Break; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 47.2 °C117 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ BNU 011 Performance Polyolefin
ExxonMobil Exxtral™ H1025W Performance Polyolefin
ExxonMobil Exxtral™ BMV 102W Performance Polyolefin
Borealis Borcom™ WE007AE Polypropylene

PEX99389 / 175625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.