MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Mirel™ P1003 is a general purpose injection molding material with high modulus.

Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and closures, and disposable items such as forks, spoons, knives, tubs, trays, jars, and consumer product applications.

About Mirel Bioplastics

Mirel is a family of bioplastic materials that have physical properties comparable to petroleum-based resins, yet are both biobased and biodegradable in natural soil and water environments, home composting systems, and industrial composting facilities, where these facilities are available. The rate and extent of Mirel's biodegradablility will depend on the size and shape of the articles made from it. However, like nearly all bioplastics and organic matter, Mirel is not designed to biodegrade in conventional landfills.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Polyhydroxyalkanoate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0125 - 0.0155 cm/cm0.0125 - 0.0155 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.0 MPa3630 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 3.00 GPa435 ksiASTM D638
Flexural Strength 40.0 MPa5800 psiASTM D790 A
Flexural Modulus 2.00 GPa290 ksiASTM D790 A
Izod Impact, Notched 0.260 J/cm0.487 ft-lb/inASTM D256 A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FASTM D648 B
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM D648 B
Vicat Softening Point 124 °C255 °FASTM 1525 B10
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 175 - 180 °C347 - 356 °FReverse Temperature Profile
Middle Barrel Temperature 170 - 175 °C338 - 347 °F
Front Barrel Temperature 165 - 170 °C329 - 338 °F
Nozzle Temperature 165 - 170 °C329 - 338 °F
Melt Temperature 160 - 165 °C320 - 329 °F
Mold Temperature 55.0 - 65.0 °C131 - 149 °F(A/B)
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Desiccant
Back Pressure <= 3.45 MPa<= 500 psiLow
Screw Speed <= 200 rpm<= 200 rpmSlow
 
Descriptive Properties
2nd Stage Pressure<30%of 1st Stage Pressure (Low)
Equipment Recommendation: Non-Return ValveStandard Check Ring
Equipment recommendation: Screw Profile2.2:1 to 2.6:1Low Shear GP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Telles Mirel™ I6003rp Biobased PHA Polymeric Modifier
Telles Mirel™ P5001 Film Grade PHA Bioplastic
Telles Mirel™ P1004 Injection Molding Grade PHA Bioplastic
Telles Mirel™ I6001 Biobased Polymeric Modifier
Overview of materials for Polystyrene, Extrusion Grade

PMETAA9670 / 150416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.