MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Copolymer CP0436C30L1 Calcium Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Calcium Carbonate (CaCO3) Filler

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inMD; ASTM D955
Melt Flow 10 g/10 min10 g/10 minASTM D1238
Ash 30 %30 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6262ASTM D785
Tensile Strength at Break 15.0 MPa2180 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 60 %60 %ASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Tensile Modulus 1.60 GPa232 ksiASTM D638
Flexural Strength 25.0 MPa3630 psiASTM D790
Flexural Modulus 1.300 GPa188.5 ksiASTM D790
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 52.2 °C126 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.1 °C196 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Aclo Accutech Polypropylene Copolymer CP0436C30L Calcium Reinforced
Aclo Accutech Polypropylene Copolymer CP0437C30L Calcium Reinforced
Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced

PACLO109 / 22364

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.