MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.53 - 1.90 g/cc0.0553 - 0.0686 lb/in³Average value: 1.72 g/cc Grade Count:32
Filler Content 50.0 %50.0 %Average value: 50.0 % Grade Count:5
Water Absorption 0.0100 - 0.0200 %0.0100 - 0.0200 %Average value: 0.0187 % Grade Count:8
Water Absorption at Saturation 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:8
Linear Mold Shrinkage 0.000500 - 0.0100 cm/cm0.000500 - 0.0100 in/inAverage value: 0.00232 cm/cm Grade Count:23
Linear Mold Shrinkage, Transverse 0.00300 - 0.00850 cm/cm0.00300 - 0.00850 in/inAverage value: 0.00582 cm/cm Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121 - 123121 - 123Average value: 123 Grade Count:6
Tensile Strength, Ultimate 36.5 - 375 MPa5300 - 54400 psiAverage value: 162 MPa Grade Count:30
 94.0 - 179.953 MPa
@Temperature -40.0 - 120 °C
13600 - 26100.0 psi
@Temperature -40.0 - 248 °F
Average value: 142 MPa Grade Count:3
Elongation at Break 0.400 - 2.20 %0.400 - 2.20 %Average value: 1.34 % Grade Count:29
 0.950 - 0.950 %
@Temperature -40.0 - 4.44 °C
0.950 - 0.950 %
@Temperature -40.0 - 40.0 °F
Average value: 0.950 % Grade Count:2
Modulus of Elasticity 9.65 - 42.1 GPa1400 - 6100 ksiAverage value: 19.7 GPa Grade Count:19
 21.4427 - 21.4427 GPa
@Temperature -40.0 - -40.0 °C
3110.05 - 3110.05 ksi
@Temperature -40.0 - -40.0 °F
Average value: 21.4 GPa Grade Count:2
Flexural Yield Strength 57.9 - 500 MPa8400 - 72500 psiAverage value: 248 MPa Grade Count:31
 269.585 - 269.585 MPa
@Temperature -40.0 - -40.0 °C
39100.1 - 39100.1 psi
@Temperature -40.0 - -40.0 °F
Average value: 270 MPa Grade Count:2
Flexural Modulus 10.3 - 39.2 GPa1500 - 5690 ksiAverage value: 17.0 GPa Grade Count:32
 9.55 - 18.6848 GPa
@Temperature -40.0 - 120 °C
1390 - 2710.04 ksi
@Temperature -40.0 - 248 °F
Average value: 15.7 GPa Grade Count:3
Izod Impact, Notched 0.587 - 3.68 J/cm1.10 - 6.90 ft-lb/inAverage value: 1.54 J/cm Grade Count:15
 0.700 - 3.7373 J/cm
@Temperature -40.0 - -20.0 °C
1.31 - 7.0015 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 2.22 J/cm Grade Count:3
Izod Impact, Unnotched 2.56 - 5.34 J/cm4.80 - 10.0 ft-lb/inAverage value: 3.65 J/cm Grade Count:7
Izod Impact, Notched (ISO) 6.00 - 25.0 kJ/m²2.86 - 11.9 ft-lb/in²Average value: 13.8 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 30.0 - 46.0 kJ/m²14.3 - 21.9 ft-lb/in²Average value: 36.3 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.20 - 4.50 J/cm²5.71 - 21.4 ft-lb/in²Average value: 3.05 J/cm² Grade Count:6
 1.20 - 3.00 J/cm²
@Temperature -40.0 - -20.0 °C
5.71 - 14.3 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 1.80 J/cm² Grade Count:2
Charpy Impact, Notched 0.600 - 2.80 J/cm²2.86 - 13.3 ft-lb/in²Average value: 1.14 J/cm² Grade Count:13
 0.600 - 0.600 J/cm²
@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.600 J/cm² Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10.0 - 2.00e+16 ohm-cm10.0 - 2.00e+16 ohm-cmAverage value: 5.65e+15 ohm-cm Grade Count:17
Surface Resistance 1000 - 8.00e+15 ohm1000 - 8.00e+15 ohmAverage value: 1.60e+15 ohm Grade Count:4
Dielectric Constant 3.80 - 5.003.80 - 5.00Average value: 4.27 Grade Count:11
Dielectric Strength 12.0 - 26.0 kV/mm305 - 660 kV/inAverage value: 16.3 kV/mm Grade Count:11
Dissipation Factor 0.00100 - 0.005000.00100 - 0.00500Average value: 0.00218 Grade Count:11
Comparative Tracking Index 125 - 250 V125 - 250 VAverage value: 164 V Grade Count:12
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 45.0 µm/m-°C3.89 - 25.0 µin/in-°FAverage value: 18.4 µm/m-°C Grade Count:5
CTE, linear, Transverse to Flow 10.0 - 61.0 µm/m-°C5.56 - 33.9 µin/in-°FAverage value: 38.0 µm/m-°C Grade Count:3
Melting Point 280 - 285 °C536 - 545 °FAverage value: 281 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 266 - 280 °C510 - 536 °FAverage value: 270 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 258 - 282 °C496 - 540 °FAverage value: 266 °C Grade Count:29
Flammability, UL94 V-0V-0Grade Count:24
Glow Wire Test 960 °C1760 °FAverage value: 960 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 70.0 - 340 °C158 - 644 °FAverage value: 239 °C Grade Count:10
Die Temperature 290 - 345 °C554 - 653 °FAverage value: 312 °C Grade Count:5
Melt Temperature 280 - 345 °C536 - 653 °FAverage value: 314 °C Grade Count:22
Mold Temperature 120 - 177 °C248 - 350 °FAverage value: 145 °C Grade Count:23
Drying Temperature 100 - 150 °C212 - 302 °FAverage value: 141 °C Grade Count:21
Moisture Content 0.0200 - 0.0400 %0.0200 - 0.0400 %Average value: 0.0267 % Grade Count:9
Injection Pressure 30.0 - 103 MPa4350 - 15000 psiAverage value: 75.5 MPa Grade Count:17

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded

O4515 / 78342

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.