MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Adstif HA5034 Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif HA5034 is a high crystallinity polypropylene homopolymer, which features an extremely high stiffness, high gloss and maintaining mechanical properties even at high temperatures. Adstif HA5034 is selected by customers for use in the production of stiff injection moulded articles where high rigidity is needed. Typical applications of HA5034 include food packaging containers, housewares, small appliances and technical parts. It is typically used by customers in small appliances and automotive compounding applications where high rigidity and very good thermal characteristics are required. Adstif HA5034 is used in food contact.

Product Features: Very high long term heat resistance and High HDT/ High Stiffness/High Crystallization Temperature/High surface hardness/ Good pigment dispersion

Typical Applications: Small appliances and technical parts/Rice cooker case/Microwave oven/Electric Kettle /Auto compound/Heater case/Food packaging containers/Housewares

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
14 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 40.2 MPa5830 psiASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Modulus 2.16 GPa313 ksiASTM D790
Izod Impact, Notched 0.196 J/cm
@Temperature 23.0 °C
0.367 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Formosa Plastics Formolene® 5140L Homopolymer Polypropylene

PMIRAF34 / 183255

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.