MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.67 g/cc0.0603 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.0 - 1.4 %1.0 - 1.4 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.1 - 4.7 %4.1 - 4.7 %ISO 62
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inrestricted
Melt Flow 41.75 g/10 min
@Load 5.00 kg,
Temperature 275 °C
41.75 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 110 MPa16000 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 1.8 %1.8 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 11.0 GPa1600 ksiISO 527-1/-2
Flexural Strength 165 MPa23900 psiat max force; ISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Izod Impact, Notched (ISO)  2.50 kJ/m²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 4.50 kJ/m²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.250 J/cm²
@Temperature 23.0 °C
1.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 - 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
22.2 - 33.3 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
CTE, linear, Transverse to Flow 40.0 - 50.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
22.2 - 27.8 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°F
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°FDIN 52612
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 149 °C300 °Ffor 50% loss of tensile strength after 20000hr
 167 °C333 °Ffor 50% loss of tensile strength after 5000hr
 200 °C392 °F
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FISO 75-1/-2
Flammability, UL94  V-2
@Thickness >=0.750 mm
V-2
@Thickness >=0.0295 in
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 310 °C554 - 590 °FInjection-molding/Extrusion
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection-molding
 
Descriptive Properties
ColorGR 22866
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
BASF Ultramid® A3UG5 BK 23260 25% Glass Filled PA66 (Dry)
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry)

PBASG0328 / 131961

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.