MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PP-GF25-0403 P10/10 PP, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Material code according to ISO 1043-1: PP
PP with 25% ash content

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.3 %2.3 %5mm/min; ISO 527-2/1A
Tensile Modulus 6.40 GPa928 ksi1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 30.0 - 70.0 °C86.0 - 158 °FCavity temperature
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 220 - 230 °C428 - 446 °F
Zone 2 230 - 240 °C446 - 464 °F
Zone 3 240 - 250 °C464 - 482 °F
Zone 4 250 °C482 °F
Die Temperature 240 - 250 °C464 - 482 °F
Melt Temperature 230 - 270 °C446 - 518 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 4.00 hour4.00 hour
Moisture Content 0.20 %0.20 %Necessary low maximum residual
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 40.0 - 80.0 MPa5800 - 11600 psi
Back Pressure 3.00 MPa435 psi
Screw Speed  25 rpm
@Diameter 75.0 mm
25 rpm
@Diameter 2.95 in
 35 rpm
@Diameter 55.0 mm
35 rpm
@Diameter 2.17 in
 50 rpm
@Diameter 40.0 mm
50 rpm
@Diameter 1.57 in
Hot-Working Temperature 230 - 270 °C446 - 518 °F
 
Descriptive Properties
Heat stabilized/stable to heatYes
Injection speedslow
Longer pre-drying times/storageCan be stored in standard conditions until processed.
Pre-dryingDrying is not normally required with proper storage
Special InformationMechanical values per injection molded samples

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced
Aclo Accutech Polypropylene Copolymer CP0436G30CL Glass Reinforced
A. Schulman Diamond NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant

PHCR184 / 158753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.