MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitting applications.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³natural resin; ASTM D792
Environmental Stress Crack Resistance >= 500 hour>= 500 hourF0; Compression molded parts prepared according to ASTM D 1928, condition A.; ASTM D1693
High Load Melt Index 44 g/10 min
@Load 21.6 kg,
Temperature 190 °C
44 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Melt Index of Compound 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4444Compression molded parts per ASTM D 1928 Procedure C.; ASTM D2240
Tensile Strength at Break 15.5 MPa2250 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Tensile Strength, Yield 11.0 MPa1600 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Elongation at Break 800 %800 %Compression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Flexural Modulus 0.310 GPa45.0 ksiCompression molded parts prepared according to ASTM D 1928, method 1, procedure B.; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -100 °C<= -148 °FCompression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DFDC-7525 NT High Density Polyethylene Resin
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Dow ELITE™ 5100G Enhanced Polyethylene Resin
INEOS Styrolution Terluran® GP-22 ABS

PDOW1371 / 30589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.