MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 899 X 141392 C NS Acetal (POM); ESD Protection - Permanently Anti-static - FDA Compliant Ingredients - APWA Plus (All Polymeric Wear Alloy) - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D 792
Linear Mold Shrinkage 0.020 - 0.030 cm/cm
@Thickness 3.20 mm
0.020 - 0.030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.8 MPa6500 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.59 GPa230 ksiASTM D 638
Flexural Strength 55.2 MPa8000 psiASTM D 790
Flexural Modulus 1.65 GPa240 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.20 mm
2.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 9.90e+10 ohm-cm1.00e+9 - 9.90e+10 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 218 °C360 - 425 °F
Mold Temperature 79.4 - 107 °C175 - 225 °F
Drying Temperature 121 °C
@Time 7200 sec
250 °F
@Time 2.00 hour
Moisture Content 0.15 %0.15 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP C 2500 FR A BLACK Polycarbonate/ABS Alloy (PC/ABS), ESD Protection - Electrically Conductive - Flame Retardant - Preliminary Datasheet
RTP Company RTP 899 X 141392 A NS Acetal (POM); ESD Protection - Permanently Anti-static - FDA Compliant Ingredients
RTP Company RTP 399 X 150726 A Polycarbonate (PC), Flame Retardant - Preliminary Datasheet
RTP Company PermaStat PLUS® 600 FR Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Static Dissipative - Flame Retardant - Preliminary Datasheet
Saint-Gobain Tygon® Chemfluor® Convoflex™ Spiral Designed Tubing Aids in Self-flushing and Cleaning

PQZRA33363 / 205819

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.