MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 79A Polyurethane, MDI Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccat processing temp, BAYTEC® XL 9611
 1.01 g/cc1.01 g/ccat processing temp, BAYTEC® XL B
 1.16 g/cc1.16 g/ccat processing temp, BAYTEC® 30BV29
 1.21 g/cc1.21 g/ccat processing temp, DESMODUR® 30BV30
Viscosity 30 cP30 cPat processing temp, BAYTEC® XL B
 80 cP80 cPat processing temp, BAYTEC® XL 9611
 650 cP650 cPat processing temp, BAYTEC® 30BV29
 2100 cP2100 cPat processing temp, DESMODUR® 30BV30
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979DIN 53505
Tensile Strength at Break 26.8 MPa3890 psiDIN 53504
Elongation at Break 673 %673 %DIN 53504
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
DIN 53504
300% Modulus 6.20 MPa
@Strain 300 %
899 psi
@Strain 300 %
DIN 53504
Resilience 5050[%]
Tear Strength 38.4 kN/m219 pliISO 34-1
Abrasion 4949[mm3]; ISO 4649
Compression Set 52 %
@Temperature 70.0 °C,
Time 86400 sec
52 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FDESMODUR® 30BV30
 30.0 °C86.0 °FBAYTEC® XL 9611
 45.0 °C113 °FBAYTEC® XL B
 70.0 °C158 °FBAYTEC® 30BV29
Mold Temperature 25.0 °C77.0 °F
 
Descriptive Properties
AppearanceliquidDESMODUR® 30BV30
 solidBAYTEC® 30BV29
 solidBAYTEC® XL 9611
 solidBAYTEC® XL B
Content100Baytec® 20BV29
 2.5Baytec® XL B
 4.8Baytec® XL9611
 56.1Desmodur® 30BV30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 62A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 88A Polyurethane, MDI Ester
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 72A Polyurethane, MDI Ester
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 73A Polyurethane, MDI PPG
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 91A Polyurethane, MDI Ester

PCOVEST0308 / 202091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.