MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Armacell Ensolite™ ECF-400 EPDM crushed foam
Categories: Other Engineering Material; Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Super soft EPDM crushed (semi-closed cell) foam.
  • UL 94 HBF listed for flame
  • Excellent resistance to ozone, weathering and heat
  • Manufacture in continuous rolls

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 - 0.128 g/cc0.00231 - 0.00463 lb/in³ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 5.0 - 105.0 - 10ASTM D2240
Tensile Strength >= 0.103 MPa>= 15.0 psiASTM D412, Die A
Elongation at Break >= 200 %>= 200 %ASTM D412
Compressive Strength <= 0.00689 MPa
@Strain 25 %
<= 1.00 psi
@Strain 25 %
ASTM D1056
Tear Strength >= 0.351 kN/m>= 2.00 pliDie C; ASTM D624
Compression Set <= 35 %
@Strain 50 %
<= 35 %
@Strain 50 %
ASTM D1056
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FIntermittent; ASTM D1056
Minimum Service Temperature, Air -56.7 °C-70.0 °FASTM D1056
Flammability, UL94 HB
@Thickness 3.30 mm
HB
@Thickness 0.130 in
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
FlammabilityPassFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Armacell Ensolite™ EF0 EPDM crushed foam
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding

PARMD061 / 186672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.