Product Description: AA53-003 is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds the AASHTO M294 requirement. Availability: Latin America, North America and South America Additive: - Thermal Stabilizer: Yes
- Antistatic: No
Applications: - Drainage Pipes
- Food packaging
- High Drainage Pipe
Information provided by ExxonMobil Chemical |