MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® RA3540 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes: Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.64 g/cc2.64 g/cc
Bulk Density 0.660 g/cc0.0238 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.6 MPa2410 psi
Elongation at Break 350 %350 %
 
Descriptive Properties
PTFE Content, %60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® PA3540LT 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound
Polikim EFALON® B-40 PTFE, 40% Bronze Filled
AGC Fluon® FC 444 PTFE, 40% Bronze Powder Filled
AGC FC 482 PTFE, 55% Bronze/ 5% Moly
AGC FC 444 PTFE, 40% Bronze

PAGC73 / 23032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.