Physical Properties | Metric | English | Comments |
---|
Density | 1.40 g/cc @Temperature 23.0 °C | 0.0506 lb/in³ @Temperature 73.4 °F |
Water Absorption | 0.50 % @Temperature 23.0 °C | 0.50 % @Temperature 73.4 °F |
Linear Mold Shrinkage | 0.010 cm/cm @Time 900 sec | 0.010 in/in @Time 0.250 hour |
Linear Mold Shrinkage, Transverse | 0.0030 cm/cm @Time 900 sec | 0.0030 in/in @Time 0.250 hour |
|
Mechanical Properties | Metric | English | Comments |
---|
Film Tensile Strength at Yield, MD | 150 MPa | 21800 psi |
Film Tensile Strength at Yield, TD | 200 MPa | 29000 psi |
Film Elongation at Break, MD | >= 200 % | >= 200 % |
Film Elongation at Break, TD | 140 % | 140 % |
Modulus of Elasticity | 3.60 GPa @Temperature 23.0 °C | 522 ksi @Temperature 73.4 °F |
| 4.30 GPa @Temperature 23.0 °C | 624 ksi @Temperature 73.4 °F |
Coefficient of Friction, Static | 0.40 | 0.40 |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Constant | 2.9 @Frequency 2.40e+8 Hz, Temperature 23.0 °C | 2.9 @Frequency 2.40e+8 Hz, Temperature 73.4 °F |
| 2.9 @Frequency 9.30e+9 Hz, Temperature 23.0 °C | 2.9 @Frequency 9.30e+9 Hz, Temperature 73.4 °F |
| 3.2 @Frequency 1e+6 Hz, Temperature 23.0 °C | 3.2 @Frequency 1e+6 Hz, Temperature 73.4 °F |
| 3.3 @Frequency 50 Hz, Temperature 23.0 °C | 3.3 @Frequency 50 Hz, Temperature 73.4 °F |
| 3.3 @Frequency 1000 Hz, Temperature 23.0 °C | 3.3 @Frequency 1000 Hz, Temperature 73.4 °F |
| 3.6 @Frequency 50 Hz, Temperature 150 °C | 3.6 @Frequency 50 Hz, Temperature 302 °F |
Dielectric Strength | 450 kV/mm @Temperature 23.0 °C | 11400 kV/in @Temperature 73.4 °F |
| 135 kV/mm @Frequency 50 Hz, Temperature 150 °C | 3430 kV/in @Frequency 50 Hz, Temperature 302 °F |
| 150 kV/mm @Frequency 50 Hz, Temperature 23.0 °C | 3810 kV/in @Frequency 50 Hz, Temperature 73.4 °F |
|
Optical Properties | Metric | English | Comments |
---|
Haze | 25 % | 25 % |
|
Descriptive Properties |
---|
Applications | Adhesive films |
| Adhesive films |
| Adhesive films |
| Adhesive tapes |
| Adhesive tapes |
| Adhesive tapes |
| Building insulation |
| Building insulation |
| Building insulation |
| Carrier film in veneer- and furniture presses |
| Carrier film in veneer- and furniture presses |
| Carrier film in veneer- and furniture presses |
| Coating |
| Coating |
| Coating |
| Collar stiffeners |
| Collar stiffeners |
| Collar stiffeners |
| Decorative films |
| Decorative films |
| Decorative films |
| Drum skins |
| Drum skins |
| Drum skins |
| Electrical insulation |
| Electrical insulation |
| Electrical insulation |
| Film for production of cast films |
| Film for production of cast films |
| Film for production of cast films |
| Film for production of GRP-products |
| Film for production of GRP-products |
| Film for production of GRP-products |
| Films for industrial applications |
| Films for industrial applications |
| Films for industrial applications |
| Flexible printed circuits |
| Flexible printed circuits |
| Flexible printed circuits |
| Gaskets and gasket inserts |
| Gaskets and gasket inserts |
| Gaskets and gasket inserts |
| Gloss laminations |
| Gloss laminations |
| Gloss laminations |
| Insulation tapes |
| Insulation tapes |
| Insulation tapes |
| Laminating |
| Laminating |
| Laminating |
| Membranes |
| Membranes |
| Membranes |
| Metallizing |
| Metallizing |
| Metallizing |
| Printing |
| Printing |
| Printing |
| Release |
| Release |
| Release |
| Reprography |
| Reprography |
| Reprography |
| Soundproofing and thermal insulation components |
| Soundproofing and thermal insulation components |
| Soundproofing and thermal insulation components |
| Stiffening |
| Stiffening |
| Stiffening |
| Tape measures |
| Tape measures |
| Tape measures |
| Transfer film |
| Transfer film |
| Transfer film |
| Transformers and coils |
| Transformers and coils |
| Transformers and coils |
Conductivity of Aqueous Extract (µS/cm) | 2 |
F5-value (MPa) | 105 |
| 105 |
Frigen Extract (%) | 0.05 |
Trichloroethylene- Extract (%) | 0.2 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.