MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celstran® PP-GF50-02- Natural PP, 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 50% Glass Fiber Filler

Material Notes: 50% long strand glass fiber chemically coupled polypropylene, Natural

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Density 1.33 g/cc0.0480 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 121 MPa17500 psiASTM D638
 148 MPa21500 psi5mm/min; ISO 527-2/1A
Elongation at Break 1.4 %1.4 %ASTM D638
 1.9 %1.9 %5mm/min; ISO 527-2/1A
Tensile Modulus 11.0 GPa1600 ksiASTM D638
 11.6 GPa1680 ksi50mm/min; ISO 527-2/1A
Flexural Strength 193 MPa28000 psiASTM D790
 252 MPa36500 psiISO 178
Flexural Modulus 9.58 GPa1390 ksiASTM D790
 12.0 GPa1740 ksiISO 178
Izod Impact, Notched 2.99 J/cm5.60 ft-lb/inASTM D256
Charpy Impact, Notched 4.40 J/cm²20.9 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C310 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 70.0 °C104 - 158 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 220 - 230 °C428 - 446 °F
Zone 2 220 - 230 °C428 - 446 °F
Zone 3 230 - 250 °C446 - 482 °F
Zone 4 230 - 250 °C446 - 482 °F
Die Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 230 - 250 °C446 - 482 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 hour2.00 hour
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF50-02-Black PP, 50% Glass Reinforced
Asahi Kasei Thermylene® P6-50FG-0100 PP-GF50
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled
Celanese Celstran® PP-GF50-03-Black PP, 50% Glass Reinforced
LG Chemical LUPOL GP2150 PP+GF15%

PHCQ233 / 178688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.