MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 2263 Polyetheretherketone (PEEK), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D 792
Additive Loading 20 %20 %Primary Additive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.8 MPa13900 psiASTM D 638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ASTM D 638
Tensile Modulus 4.55 GPa660 ksiASTM D 638
Flexural Strength 172 MPa25000 psiASTM D 790
Flexural Modulus 4.76 GPa690 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 4.81 J/cm
@Thickness 3.20 mm
9.00 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
Shielding Effectiveness  88 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
88 dB
@Thickness 0.0787 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 89 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
89 dB
@Thickness 0.0787 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 89 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
89 dB
@Thickness 0.0787 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 91 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
91 dB
@Thickness 0.0787 in,
Frequency 1e+9 Hz
ASTM D 4935
 92 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
92 dB
@Thickness 0.0787 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 95 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
95 dB
@Thickness 0.0787 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 97 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
97 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 100 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
100 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 100 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
100 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 102 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
102 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 104 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
104 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 105 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
105 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 349 - 399 °C660 - 750 °F
Mold Temperature 163 - 218 °C325 - 425 °F
Drying Temperature 149 °C
@Time 10800 sec
300 °F
@Time 3.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 362 UV BLACK Polycarbonate (PC); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized

PQZTA20591 / 159308

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.