MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more rapidly at elevated temperatures. It offers a very convenient one to one mix ratio, by weight or volume. EP21LVSP6 is particularly well conceived for specialty applications where the combination of a long open time, low viscosity and excellent physical properties are all vital to an application. The system also has very good chemical resistance to water, oil, fuel, acids and bases. EP21LVSP6 bonds well to a variety of substrates, including metals, composites, glass, ceramics, rubbers and plastics. It has very good physical strength properties as well as being a good electrical insulator. It has a service temperature range of -60°F to +250°F. The color of Part A is clear and Part B is amber clear. This system can be used in aerospace, electronic, electrical, optical and other specialty applications where high performance properties combined with a long pot life and low viscosity are desirable. As one would expect with this kind of system, it has very low exotherm and can be used for large castings.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio
  • Low viscosity for ease of application
  • Exceptionally long open time
  • High bonding strength to a wide variety of substrates
  • Magnificent electrical insulation properties
  • Little exotherm; suitable for large castings

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 1500 - 3000 cP1500 - 3000 cPPart A
 5000 - 8000 cP5000 - 8000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 70>= 70
Tensile Strength at Break >= 48.3 MPa
@Temperature 23.9 °C
>= 7000 psi
@Temperature 75.0 °F
Shear Strength >= 17.2 MPa>= 2500 psiAl/Al, Tensile lap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 2.8
@Frequency 60 Hz,
Temperature 25.0 °C
2.8
@Frequency 60 Hz,
Temperature 77.0 °F
Dielectric Strength 17.7 kV/mm
@Thickness 3.17 mm
450 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 - 55.0 µm/m-°C27.8 - 30.6 µin/in-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  4320 - 14400 min
@Temperature 93.3 °C
72.0 - 240 hour
@Temperature 200 °F
 4320 - 18000 min
@Temperature 23.9 °C
72.0 - 300 hour
@Temperature 75.0 °F
Pot Life 3.0 - 5.0 min3.0 - 5.0 min100 gram mass
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Master Bond EP21FRNS-2 Two Component Flame Retardant Epoxy
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound
Master Bond EP21TDCS Silver Filled Electrically Conductive Epoxy Compound

PMASTB314 / 149561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.