MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Delpet® 670N Acrylic Molding Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: 670N is a solvent-resistant grade, virtually unaffected by painting, printing, and antistatic treatment. General Delpet® qualities include attractive transparency, elegant luster and color brightness, excellent weather resistance, surface hardness, excellent chemical resistance, superior electrical resistance and insulation properties, and superior machinability.

Key Words: PMMA; Polymethylmethacrylate; Polymethyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %details not reported; ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
Melt Flow 4.0 g/10 min4.0 g/10 minCondition L; ASTM D1238
 8.0 g/10 min8.0 g/10 minCondition I; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ASTM D785
Tensile Strength, Ultimate 71.0 MPa10300 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Yield Strength 110 MPa16000 psiASTM D790
Flexural Modulus 3.30 GPa479 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmASTM D257
Dielectric Constant  3.0
@Frequency 40.0 - 50.0 Hz
3.0
@Frequency 40.0 - 50.0 Hz
ASTM D150
 4.0
@Frequency 60 Hz
4.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inShort-term; 4 kV/s; ASTM D149
Dissipation Factor  0.020
@Frequency 40.0 Hz
0.020
@Frequency 40.0 Hz
ASTM D150
 0.040
@Frequency 50 Hz
0.040
@Frequency 50 Hz
ASTM D150
 0.060
@Frequency 60 Hz
0.060
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
33.3 µin/in-°F
@Temperature 68.0 °F
ASTM D257
Specific Heat Capacity 1.46 J/g-°C0.349 BTU/lb-°F
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 84.0 °C183 °FHeat Distortion Temp
 84.0 °C183 °FDeflection Temp; Load not reported; ASTM D648
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49
Transmission, Visible 93 %93 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GEHR Plastics PVC-U Polyvinylchloride
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for Polycarbonate, Molded
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded

PLAA77 / 49810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.