MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Primacor® 1321 Ethylene Acrylic Acid (EAA)
Categories: Polymer; Film; Thermoplastic; Ethylene Acrylic Acid

Material Notes: PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1321 is used as adhesive or sealant layer in Flexible packaging structures. It complies with FDA regulation 21 CFR 177.1310 (b) for food packaging.

Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³
Thickness 60.0 microns2.36 mil
Melt Flow 2.5 g/10 min
@Load 2.16 kg
2.5 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 20.3 MPa2940 psiMolded property
Film Tensile Strength at Yield, MD 9.40 MPa1360 psi
Film Tensile Strength at Yield, TD 9.20 MPa1330 psi
Tensile Strength, Yield 9.80 MPa1420 psiMolded property
Film Elongation at Break, MD 470 %470 %
Film Elongation at Break, TD 570 %570 %
Elongation at Break 660 %660 %Molded value
Elmendorf Tear Strength MD 255 g255 g
Elmendorf Tear Strength TD 305 g305 g
Elmendorf Tear Strength, MD 4.30 g/micron109 g/mil
Elmendorf Tear Strength, TD 5.10 g/micron130 g/mil
Dart Drop 6.80 g/micron173 g/mil
Film Tensile Strength at Break, MD 32.4 MPa4700 psi
Film Tensile Strength at Break, TD 32.8 MPa4760 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.3 °C195 °F
 
Optical PropertiesMetricEnglishComments
Haze 3.7 %3.7 %
Gloss 75 %75 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 191 °C376 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Primacor® 3330 Ethylene Acrylic Acid (EAA)
Dow Primacor® 5990I Ethylene Acrylic Acid (EAA)
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Dow Primacor® 3460 Ethylene Acrylic Acid (EAA)
Dow Primacor® 4608 Ethylene Acrylic Acid (EAA)

PDW520 / 34589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.