MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: 100% Polystyrene.

Pre-expansion

High density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular production. It is the unique design of polystyrene chains that gives the high strength advantages to Jackocell® R311 in pre-expansion

Shape Moulding

Fast molding cycles, good fusion, and easy to reach good surface. The additional broad moulding window further reduces waste material and maintains a high quality to the extent that it can be recognized long term on productivity and financial earnings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0140 g/cc0.000506 lb/in³1.2 minute residence time pre-expander
 0.0170 g/cc0.000614 lb/in³2.4 minute residence time pre-expander
 0.0200 g/cc0.000723 lb/in³0.9 minute residence time pre-expander
 0.0280 g/cc0.00101 lb/in³0.5 minute residence time pre-expander
Water Absorption 4.6 %4.6 %13-20 hour silo ageing time; Volume%
Bead Size 0.700 - 1.00 mm0.0276 - 0.0394 in
 
Chemical PropertiesMetricEnglishComments
Blowing Agent Content >= 6.0 %>= 6.0 %Pentane
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 0.333 MPa48.3 psi16 hour silo aging time, 20 kg/m^3
 0.340 MPa49.3 psi32 hour silo aging time, 20 kg/m^3
 0.346 MPa50.2 psi48 hour silo aging time, 20 kg/m^3
 0.352 MPa51.1 psi64 hours silo aging time, 20 kg/m^3
Compressive Strength 0.120 MPa17.4 psi16 hour silo aging time, 20 kg/m^3
 0.124 MPa17.9 psi32 hour silo aging time, 20 kg/m^3
 0.127 MPa18.5 psi48 hour silo aging time, 20 kg/m^3
 1.32 MPa191 psi64 hours silo aging time, 20 kg/m^3
 
Descriptive Properties
Coefficient of Variation (%), max15
Molding Cycle Time (sec)10064 hours silo aging time, 20 kg/m^3
 11048 hour silo aging time, 20 kg/m^3
 14032 hour silo aging time, 20 kg/m^3
 2106 hour silo aging time, 20 kg/m^3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical R160 EPS, Flame Retardant
LG Chemical B160 EPS, Non-Flame Retardant
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Sekisui PIOCELAN SP-50D Moldable Polymer Foam
LG Chemical R320 EPS, Flame Retardant

PJACK001 / 85567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.