MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Inno-Comp INNOPOL® CS 1-3610 UW Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: INNOPOL® CS 1-3610 UW is a white colored, flame retarded and UV-stabilized polypropylene homopolymer compound.

INNOPOL® CS 1-3610 UW is recommended for producing electric articles by injection molding.

All information provided by INNO-COMP.

Key Words: PP-H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc
@Temperature 23.0 °C
0.0350 lb/in³
@Temperature 73.4 °F
ISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 8.0 %8.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1.65 GPa239 ksi2 mm/min; ISO 527-1,-2
Flexural Modulus 1.50 GPa218 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO)  3.50 kJ/m²
@Temperature -20.0 °C
1.67 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °FISO 75-1,-2
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® 5000/V0-AF-EP Self Extinguishing Polypropylene Copolymer, Flame Resistant
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene
LyondellBasell Hostacom™ AE716BC Polypropylene Homopolymer
LG Chemical SEETEC H7511 Polypropylene, Homopolymer

PINNO014 / 82675

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.