MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Features and Typical Applications
Ability to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in harsh environments. Typical applications include sensors, transformers, power supplies, and rectifiers.

Emerson & Cuming 4952/25 Stycast® Two-Component Silicone High Service Temp Encapsulant
  • Thermally Conductive
  • Poor Chemical Resistance
  • Filled
  • Mix Ratio by Weight = 100:0.4
Cure Type: Room Temp or Heat Bonding Type: Silicone

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³
Viscosity 35000 cP
@Temperature 25.0 °C
35000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.2
@Frequency 1e+6 Hz
5.2
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 162 µm/m-°C
@Temperature 20.0 °C
90.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 360 min4.00 - 6.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy

PEMERS15 / 35707

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.