MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Miracll E175DL Thermoplastic Polyurethane (TPUR), Polyester Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Excellent processing properties, fast setting time, no migration, good UV resistance, excellent flowing properties. Application: phone & pad cover, belting, hose & tube, wire & cable, footwear, caster, film, coating, over-molding, etc.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D2240
Tensile Strength 55.0 MPa7980 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
100% Modulus 25.0 MPa
@Strain 100 %
3630 psi
@Strain 100 %
ASTM D412
300% Modulus 40.0 MPa
@Strain 300 %
5800 psi
@Strain 300 %
ASTM D412
Tear Strength 190 kN/m1080 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -15.0 °C5.00 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Covestro DESMODUR® LU-T75D + MOCA Polyurethane, TDI-PTMEG
Covestro DESMODUR® LU-T75D + BAYTEC® XL 1705 Polyurethane, TDI-PTMEG
Austin Novel Materials Innonen® B71D Polyester-based TPU Elastomer
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane

PMIRAC19 / 221348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.