MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil EVA 150028 Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: ExxonMobil™ EVA 150028 is a high flow, 27.6% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends.

Availability: Asia Pacific, North America, Latin America.  Additives: antiblock: no; slip: no;  thermal stabilizer: yes.  Applications: adhesives and sealants, industrial sealants, hot melt adhesives, wax blends. Forms: pellets.

Information provided by ExxonMobil.

Key Words: Escorene™ Ultra UL 7720
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
Vinyl Acetate Content 27.6 %27.6 %ExxonMobil Method
Melt Flow 150 g/10 min
@Load 2.16 kg,
Temperature 190 °C
150 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Time 15.0 sec
75
@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 19
@Time 15.0 sec
19
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 2.28 MPa330 psiASTM D638
Elongation at Break 520 %520 %ASTM D638
Flexural Modulus, 1% Secant 18.6 MPa2700 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 66.1 °C151 °FPeak; ExxonMobil Method
Vicat Softening Point 51.1 °C124 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent

PEX98943 / 238324

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.