MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® M5562 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Applications
ALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include nozzle valves and specialty injection molded parts.

Regulatory Status
M 5562 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing M 5562 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ASTM D1505
Melt Flow 6.0 g/10 min6.0 g/10 minASTM D1238
Spiral Flow 31.5 cm12.4 inSpiral channel (0.625” insert) with injection pressure of 1000 psi at 440°F.; Equistar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ASTM D2240
Tensile Strength at Break 18.2 MPa2640 psiASTM D638
Tensile Strength, Yield 29.5 MPa4280 psiCrosshead speed - 2"min.; ASTM D638
Elongation at Yield 7.0 %7.0 %Crosshead speed - 2"min.; ASTM D638
Flexural Modulus, 1% Secant 1320 MPa191000 psiCrosshead speed - 0.5" min; ASTM D790
2% Secant Modulus 1.08 GPa157 ksiCrosshead speed - 0.5" min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3620WZ Polypropylene, Injection Molding Grade
LyondellBasell Alathon® M5040 High Density Polyethylene
Flint Hills P5M4K-046 Random Copolymer Polypropylene
LyondellBasell Alathon M 5265 High Denisty Polyethylene
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade

PEQU0423 / 36866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.