MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M G18/500 Glass Bubbles
Categories: Ceramic; Glass

Material Notes: Floated series glass bubbles specially treated with coupling agents for high-tech applications. G18/500 glass bubbles have a crush strength of 500 PSI and a true density of 0.18 g/cc.

Capabilities: Temperature Resistance, Light weighting, Chemical Resistance

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.180 g/cc0.180 g/cc
Particle Size 30 - 39 µm30 - 39 µmD50, Range
 35 µm35 µmD50
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3.40 MPa493 psi
Compressive Strength 3.45 MPa500 psi
 
Descriptive Properties
AppearanceWhite, powdery
CompositionSoda-lime-borosilicate glass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M K42HS Glass Bubbles
3M K11 Glass Bubbles
3M HGS8000X Glass Bubbles
3M HGS18000 Glass Bubbles
3M HGS10000 Glass Bubbles

CMM40006 / 194897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.