MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Lucalen A2910M Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lucalen A2910M is a natural adhesive low density polyethylene copolymer with a high thermal stability. Due to the acrylic acid/acrylate copolymer (E/A) content this grade offers excellent adhesion to polar materials (i.e. epoxy resin, steel, aluminum, etc.). It is designed to be used in 2-layer anti corrosion coating as well as in wire & cable compounds. The material is available in pellet form. Applications: Coatings, Protective, Pipe Coating

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.500 g/cc>= 0.0181 lb/in³ISO 60
Density 0.927 g/cc0.0335 lb/in³ISO 1183-1
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3838ISO 868
Tensile Strength, Yield 6.00 MPa870 psiISO 527-1,-2
Tensile Modulus 0.0840 GPa12.2 ksiISO 527-1,-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.0 °C205 °FISO 11357-3
Vicat Softening Point 72.0 °C162 °FA/50N; ISO 306
 
Descriptive Properties
Comonomer AA (%)4DIN 51451
Comonomer tert-BA (%)7DIN 51451
Processing MethodExtrusion Coating, Sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2700H Low Density Polyethylene
LyondellBasell Lucalen A2540D Low Density Polyethylene
LyondellBasell Lucalen A2700M Low Density Polyethylene
LyondellBasell Lucalen A2920M Low Density Polyethylene
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer

PEQT7605 / 219242

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.