MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UBE 7034T Nylon 6/12 Monofilament (Drawing Ratio=6, Diameter 0.4 mm)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Specialties: High viscosity Nylon 6/12 Copolymer, High stretch-ability results higher line strength than 50 series, Lower moisture absorption keeps superior physical property even in the water

Applications: Small- large size sport fishing line and long line (branch line), Appearance of filament is said to be "brilliant crystal tone" and reputed in the branch line application

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Fiber Count 1510 dtex1360 denier
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 27 %27 %Knot Elongation
 31 %31 %Line Elongation
Tenacity 0.671 N/tex7.60 g/denierKnot Strength
 0.777 N/tex8.80 g/denierLine Strength
 1.94 N/tex22.0 g/denierTensile Modulus
 
Thermal PropertiesMetricEnglishComments
Shrinkage 21 %21 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Novamid® 2430J PA666
Envalior Novamid® 2420A PA666
BASF Ultramid® C3U10 PA6/66 FR (Conditioned)
AdvanSix Aegis® HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
UBE 7034B Nylon 6/12 Copolymer Film

PUBE063 / 71623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.