MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES HiFill® HIPS GF20 BK 20% Glass Filled
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Grade, Glass Filled

Material Notes: Availability: North America

Forms: Pellets

Glass Fiber Reinforcement, 20% Filler by Weight

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Water Absorption 0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.17 mm
0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 68.9 MPa10000 psiASTM D638
Elongation at Break 1.0 %1.0 %ASTM D638
Flexural Strength 96.5 MPa14000 psiASTM D790
Flexural Modulus 7.24 GPa1050 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.17 mm
1.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.14 J/cm
@Thickness 3.17 mm
4.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 17.7 kV/mm450 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.6 µm/m-°C17.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips EB6025 HIPS - High Impact Polystyrene
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled
BLUESTAR LXS 312 PPE-HIPS, 20% Mineral Filled
INEOS Styrolution PS 454N HIPS
RTP Company RTP 400 GB 20  Polystyrene (PS) Glass Bead 20%

PTPC0076 / 136014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.