MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.21 g/cc0.0376 - 0.0437 lb/in³Average value: 1.08 g/cc Grade Count:100
 0.900 - 0.900 g/cc
@Temperature 260 - 260 °C
0.0325 - 0.0325 lb/in³
@Temperature 500 - 500 °F
Average value: 0.900 g/cc Grade Count:2
Filler Content 8.00 - 9.00 %8.00 - 9.00 %Average value: 8.33 % Grade Count:3
Water Absorption 0.200 - 6.40 %0.200 - 6.40 %Average value: 2.77 % Grade Count:42
Moisture Absorption at Equilibrium 0.800 - 2.00 %0.800 - 2.00 %Average value: 1.43 % Grade Count:42
Water Absorption at Saturation 1.40 - 4.30 %1.40 - 4.30 %Average value: 2.48 % Grade Count:11
Maximum Moisture Content 0.0200 - 0.05000.0200 - 0.0500Average value: 0.0400 Grade Count:3
Linear Mold Shrinkage 0.00400 - 0.0140 cm/cm0.00400 - 0.0140 in/inAverage value: 0.00776 cm/cm Grade Count:64
 0.00700 - 0.00700 cm/cm
@Temperature 80.0 - 80.0 °C
0.00700 - 0.00700 in/in
@Temperature 176 - 176 °F
Average value: 0.00700 cm/cm Grade Count:1
Linear Mold Shrinkage, Transverse 0.00600 - 0.0140 cm/cm0.00600 - 0.0140 in/inAverage value: 0.00839 cm/cm Grade Count:23
 0.00800 - 0.00800 cm/cm
@Temperature 80.0 - 80.0 °C
0.00800 - 0.00800 in/in
@Temperature 176 - 176 °F
Average value: 0.00800 cm/cm Grade Count:1
Melt Flow 1.00 - 65.0 g/10 min1.00 - 65.0 g/10 minAverage value: 22.9 g/10 min Grade Count:57
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 69.0 - 11669.0 - 116Average value: 101 Grade Count:29
Hardness, Shore D 64.064.0Average value: 64.0 Grade Count:3
Ball Indentation Hardness 70.0 - 102 MPa10200 - 14800 psiAverage value: 86.0 MPa Grade Count:6
Tensile Strength, Ultimate 4.00 - 63.8 MPa580 - 9250 psiAverage value: 43.3 MPa Grade Count:45
Tensile Strength, Yield 27.0 - 100 MPa3920 - 14500 psiAverage value: 43.3 MPa Grade Count:59
Elongation at Break 3.10 - 230 %3.10 - 230 %Average value: 69.4 % Grade Count:81
Elongation at Yield 2.90 - 110 %2.90 - 110 %Average value: 8.25 % Grade Count:45
Modulus of Elasticity 0.900 - 5.30 GPa131 - 769 ksiAverage value: 1.99 GPa Grade Count:56
Flexural Yield Strength 32.0 - 150 MPa4640 - 21800 psiAverage value: 67.5 MPa Grade Count:78
Flexural Modulus 0.680 - 4.80 GPa98.6 - 696 ksiAverage value: 1.90 GPa Grade Count:80
Izod Impact, Notched 0.588 J/cm - NB1.10 ft-lb/in - NBAverage value: 5.88 J/cm Grade Count:39
 0.490332 - 8.0085 J/cm
@Temperature -40.0 - -18.0 °C
0.918594 - 15.003 ft-lb/in
@Temperature -40.0 - -0.400 °F
Average value: 1.36 J/cm Grade Count:7
 0.5339 - 2.50 J/cm
@Temperature -40.0 - 0.000 °C
1.000 - 4.68 ft-lb/in
@Temperature -40.0 - 32.0 °F
Average value: 1.36 J/cm Grade Count:7
 0.5339 - 2.50 J/cm
@Thickness 3.17 - 6.35 mm
1.000 - 4.68 ft-lb/in
@Thickness 0.125 - 0.250 in
Average value: 1.36 J/cm Grade Count:7
Izod Impact, Notched (ISO) 7.00 - 80.0 kJ/m²3.33 - 38.1 ft-lb/in²Average value: 53.9 kJ/m² Grade Count:17
 5.00 - 30.0 kJ/m²
@Temperature -30.0 - -30.0 °C
2.38 - 14.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 13.1 kJ/m² Grade Count:14
Izod Impact, Unnotched (ISO) 100 - 160 kJ/m²47.6 - 76.1 ft-lb/in²Average value: 120 kJ/m² Grade Count:3
 55.0 - 60.0 kJ/m²
@Temperature -30.0 - -30.0 °C
26.2 - 28.6 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 57.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 7.00 J/cm² - NB33.3 ft-lb/in² - NBAverage value: 13.8 J/cm² Grade Count:30
 0.600 J/cm² - NB
@Temperature -30.0 - -30.0 °C
2.86 ft-lb/in² - NB
@Temperature -22.0 - -22.0 °F
Average value: 5.24 J/cm² Grade Count:19
Charpy Impact, Notched 0.400 - 10.8 J/cm²1.90 - 51.4 ft-lb/in²Average value: 4.66 J/cm² Grade Count:56
 0.600 - 10.8 J/cm²
@Temperature -30.0 - -30.0 °C
2.86 - 51.4 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.83 J/cm² Grade Count:30
Puncture Energy 6.50 - 11.0 J
@Temperature -30.0 - -30.0 °C
4.79 - 8.11 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 8.75 J Grade Count:2
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 - 9.70e+15 ohm-cm1.00e+10 - 9.70e+15 ohm-cmAverage value: 7.08e+14 ohm-cm Grade Count:36
Surface Resistance 3.20e+13 - 8.30e+15 ohm3.20e+13 - 8.30e+15 ohmAverage value: 7.83e+14 ohm Grade Count:29
Dielectric Constant 2.90 - 6.702.90 - 6.70Average value: 3.52 Grade Count:30
Dielectric Strength 15.0 - 40.0 kV/mm380 - 1020 kV/inAverage value: 28.5 kV/mm Grade Count:16
Dissipation Factor 0.00770 - 0.1000.00770 - 0.100Average value: 0.0339 Grade Count:28
Comparative Tracking Index 550 - 600 V550 - 600 VAverage value: 596 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 - 140 µm/m-°C30.0 - 77.8 µin/in-°FAverage value: 96.9 µm/m-°C Grade Count:28
CTE, linear, Transverse to Flow 90.0 - 127 µm/m-°C50.0 - 70.6 µin/in-°FAverage value: 110 µm/m-°C Grade Count:8
Melting Point 220 - 224 °C428 - 435 °FAverage value: 221 °C Grade Count:15
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 190 °C176 - 374 °FAverage value: 98.9 °C Grade Count:48
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 110 °C124 - 230 °FAverage value: 72.6 °C Grade Count:66
Vicat Softening Point 91.0 - 245 °C196 - 473 °FAverage value: 133 °C Grade Count:46
Flammability, UL94 HB - V-0HB - V-0Grade Count:42
Glow Wire Test 650 - 700 °C1200 - 1290 °FAverage value: 665 °C Grade Count:7
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 280 °C464 - 536 °FAverage value: 260 °C Grade Count:3
Nozzle Temperature 216 - 260 °C420 - 500 °FAverage value: 243 °C Grade Count:7
Melt Temperature 190 - 280 °C374 - 536 °FAverage value: 248 °C Grade Count:61
Mold Temperature 10.0 - 93.0 °C50.0 - 199 °FAverage value: 61.1 °C Grade Count:61
Injection Velocity 20.0 - 65.0 mm/sec0.787 - 2.56 in/secAverage value: 44.5 mm/sec Grade Count:10
Drying Temperature 80.0 - 120 °C176 - 248 °FAverage value: 86.7 °C Grade Count:19
Moisture Content 0.0500 - 0.350 %0.0500 - 0.350 %Average value: 0.162 % Grade Count:4
Injection Pressure 30.0 - 82.7 MPa4350 - 12000 psiAverage value: 58.0 MPa Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled

O1160a / 89058

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.