MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive-Air Induction System Ducts, Boots and Bellows for Steering and Suspension, Plugs, Bumpers, Grommets, Clips, Seals, Gaskets and Weather Seals
  • Consumer-Electronic and Floor Care
  • Industrial – Seals and Gaskets
  • Tubing
Uses:
  • Appliance Components
  • Consumer Applications
  • Gaskets
  • Automotive Applications
  • Diaphrams
  • Seals
  • Automotive Under the Hood
  • Electrical Parts
  • Tubing
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant; UL JMLU2; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78782mm/ 15 sec; ISO 868
 8585Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 8.74 MPa1270 psiAir at 302°F, 168 hr; ASTM D573
 8.83 MPa1280 psiAcross Flow; ASTM D412
Tensile Stress at Strain 3.60 MPa
@Strain 100 %
522 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 475 %475 %Air at 302°F, 168 hr; ASTM D573
 490 %490 %Across Flow; ASTM D412
Tear Strength 27.0 kN/m154 pli73°C, Die C; ASTM D624
Compression Set  28 %
@Temperature 70.0 °C,
Time 79200 sec
28 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 37 %
@Temperature 125 °C,
Time 252000 sec
37 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.52.51.98 mm; ASTM D150
Dielectric Strength 26.8 kV/mm680 kV/in2.03 mm; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical with Impact  90.0 °C
@Thickness 1.00 mm
194 °F
@Thickness 0.0394 in
UL 746
 90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
UL 746
 95.0 °C
@Thickness 3.00 mm
203 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Rear Barrel Temperature 177 °C350 °F
Middle Barrel Temperature 182 °C360 °F
Front Barrel Temperature 188 °C370 °F
Nozzle Temperature 193 - 227 °C380 - 440 °F
Die Temperature 204 °C400 °FExtrusion
Melt Temperature 202 °C395 °FExtrusion
 199 - 232 °C390 - 450 °FProcessing
Mold Temperature 10.0 - 51.7 °C50.0 - 125 °FProcessing
Drying Temperature 82.2 °C180 °F
Dry Time 3 hour3 hour
Moisture Content 0.080 %0.080 %
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psiProcessing
 5.00 - 20.0 MPa725 - 2900 psiExtrusion
Clamp Pressure 41.4 - 68.9 MPa6000 - 10000 psi
Vent Depth 0.00254 cm0.00100 in
Cushion 0.317 - 0.635 cm0.125 - 0.250 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Celanese Hytrel® 5556 TPC-ET
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer

PADVA043 / 22733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.