MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

North Wood Plastics HDPE with 40% Wood Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Wood Filled

Material Notes: Data provided by North Wood Plastics, Inc.

Key Words: Wood Flour; High Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.054 g/cc0.03808 lb/in³ASTM D792
Linear Mold Shrinkage 0.0072 cm/cm0.0072 in/inASTM D955
Melt Flow 2.3 g/10 min
@Temperature 190 °C
2.3 g/10 min
@Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 16.0 MPa2320 psiASTM D638
Tensile Strength, Yield 18.0 MPa2610 psiASTM D638
Elongation at Break 4.9 %4.9 %ASTM D638
Tensile Modulus 2.70 GPa392 ksiASTM D638
Flexural Yield Strength 35.0 MPa5080 psiASTM D790
Flexural Modulus 2.40 GPa348 ksiASTM D790
Izod Impact, Notched 0.210 J/cm0.393 ft-lb/inASTM D256
Izod Impact, Unnotched 0.550 J/cm1.03 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 58.0 µm/m-°C
@Temperature 20.0 °C
32.2 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C127 °FASTM D648
Flammability, UL94 HBHB0.32 cm x 1.25 cm x 12.5 cm sample
 HBHB0.32 cm x 1.25 cm x 12.5 cm sample
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 200 °C<= 392 °FTo prevent fiber degradation.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North Wood Plastics 60 HDPE + UNIFILL (40% Wood Fiber)
North Wood Plastics HDPE with 60% Wood Fiber
GEHR Plastics ECOGEHR® WPC-30PE Composite of 70% Wood Fibers and 30% Polyethylene (PE)
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
FKuR Kunststoff Fibronlon® S 7530 Wood-Plastic Composite

PWOOD87 / 20252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.