MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® L 25 W 40 ESD PA12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inherent color of this material is black. The main features of Grilamid L 25 W 40 ESD are:
  • Anti-static
  • Highly flexible
  • Good heat stability
  • Good dimensional stability
  • Easy processing
  • Low density, low weight
Application examples: Grilamid L 25 W 40 ESD is suitable for the production of highly flexible tubes and profiles having anti-static properties for use in automotive and industrial applications.

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Water Absorption 1.1 %1.1 %ISO 62
Moisture Absorption 0.600 %0.600 %ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363conditioned, 15s; ISO 868
Tensile Strength at Break 35.0 MPa5080 psidry; ISO 527-1/-2
 35.0 MPa5080 psiconditioned; ISO 527-1/-2
Tensile Strength, Yield 25.0 MPa3630 psidry; ISO 527-1/-2
 25.0 MPa3630 psiconditioned; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %conditioned; ISO 527-1/-2
 <= 50 %<= 50 %dry; ISO 527-1/-2
Elongation at Yield 20 %20 %conditioned; ISO 527-1/-2
 20 %20 %dry; ISO 527-1/-2
Tensile Modulus 0.350 GPa50.8 ksiconditioned; ISO 527-1/-2
 0.350 GPa50.8 ksidry; ISO 527-1/-2
Charpy Impact Unnotched NBNBdry; ISO 179/1eU
 NBNBconditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NBNBdry; ISO 179/1eA
 NBNBconditioned; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+051e+05conditioned; IEC 60093
Surface Resistance 1.00e+6 ohm1.00e+6 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
Melting Point 173 °C343 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C194 - 230 °Flong term; EMS
 150 °C302 °Fshort term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AdditivesPlasticizer
AutomotiveFuel systems
Electricals & ElectronicsCables & Tubes
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
ProcessingOther Extrusion
Product AttributesFlexible
 High viscosity
Special CharacteristicsAnti-static
 High impact or impact modified
 Improved heat resistance
 Improved UV resistance (outdoor use)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman ComAlloy Comshield® 120 Copolymer Polypropylene, Electrically Conductive - Carbon Black Filled
A. Schulman ComAlloy Comshield® 104 Homopolymer Polypropylene, Electrically Conductive - Carbon Black Filled
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
Teijin Panlite® E-8715 EMS Shield Grade Polycarbonate
Teijin Panlite® EN-8515N EMS Shield Grade Polycarbonate

PGRH051 / 156760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.