MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Freudenberg S313 Silicone Elastomer (VMQ)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasoline and solvents; poor resistance to alkalis and acids.

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: BAYSOLINE®, SILASTIC® , SILPLUS®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272Original Property; ASTM D2240
 7878Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 8.30 MPa1200 psiOriginal Property; ASTM D412 Die C
 6.990 MPa1014 psiAir Aging, 70 hours; ASTM D412 Die C
Elongation at Break 378 %378 %Original Property; ASTM D412 Die C
 268.38 %268.38 %Air Aging, 70 hours; ASTM D412 Die C
Tear Strength 31.9 kN/m182 pliASTM D624 Die B
Compression Set  18 %
@Temperature 100 °C,
Time 79200 sec
18 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395 Method B
 38 %
@Temperature 150 °C,
Time 252000 sec
38 %
@Temperature 302 °F,
Time 70.0 hour
ASTM D395 Method B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -115 °C-175 °FASTM D2137
 
Descriptive Properties
ColorRed
Low Temperature BrittlenessPass, No crackASTM D2137

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Freudenberg S40 Silicone Elastomer (VMQ)
Freudenberg S315 Silicone Elastomer (VMQ)
Freudenberg S50 Silicone Elastomer (VMQ)
Freudenberg S314 Silicone Elastomer (VMQ)
Freudenberg S60 Silicone Elastomer (VMQ)

PSIMR152 / 79114

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.