MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3K BK 00464 PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: Easy flowing injection-molding grade for fast processing. Uses include highly stressed technical parts such as bearings and gear wheels; also electrically insulating parts such as terminals and cable connectors, as Fc grade suitable for food contact.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.5 - 3.1 %2.5 - 3.1 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 8.0 - 9.0 %8.0 - 9.0 %ISO 62
Viscosity Measurement 150150ISO 307
Linear Mold Shrinkage 0.0085 cm/cm0.0085 in/inrestricted
Melt Flow 129.95 g/10 min
@Load 5.00 kg,
Temperature 275 °C
129.95 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 20 %20 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 1.10 GPa160 ksiISO 527-1/-2
Izod Impact, Notched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 700 MPa102000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°F
Thermal Conductivity 0.330 W/m-K2.29 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 101 °C214 °Ffor 50% loss of tensile strength after 20000hr
 118 °C244 °Ffor 50% loss of tensile strength after 5000hr
 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection-molding
 
Descriptive Properties
ColorBK 00464
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3K BK00464 PA66 (Dry)
Celanese Zytel® ST801 NC010A PA66-HI
Envalior Stanyl® TW341-N PA46
BASF Ultramid® A3K PA66 (Dry)
Envalior Stanyl® TS300 PA46

PBASG0218 / 131851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.