MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lotte Advanced Materials Starex® TX-0510T TRABS, Unreinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes:

Information provided by Samsung Cheil Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Melt Flow 17 g/10 min
@Load 10.0 kg,
Temperature 220 °C
17 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 109109ASTM D785
Tensile Strength, Yield 45.1 MPa6540 psi5 mm/min; ASTM D638
Flexural Strength 63.7 MPa9240 psi2.8 mm/min; ASTM D638
Flexural Modulus 2.06 GPa299 ksi2.8 mm/min; ASTM D790
Izod Impact, Notched 1.27 J/cm
@Thickness 3.17 mm
2.39 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °FB/50; ISO R306
Flammability, UL94 HB
@Thickness 1.50 - 3.00 mm
HB
@Thickness 0.0591 - 0.118 in
 
Optical PropertiesMetricEnglishComments
Haze 2.8 %
@Thickness 3.20 mm
2.8 %
@Thickness 0.126 in
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.20 mm
88 %
@Thickness 0.126 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Lustran® 266 ABS, Transparent Grade
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
Lotte Advanced Materials Starex® TX-0510 TRABS, Unreinforced
Techmer ES HiFill FR® ASA FR-2A WT209
A. Schulman Diamond ABS TR-5000 Transparent

PSAMSU914 / 146731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.