MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nimonic 75, Ni-P 91-HT, ATG R, RTG 0 Superalloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes:

Cr19.5-Fe4-Ni75-Ti0.4

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.37 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  8.00 MPa
@Temperature 980 °C,
Time 3.60e+6 sec
1160 psi
@Temperature 1800 °F,
Time 1000 hour
 10.0 MPa
@Temperature 980 °C,
Time 360000 sec
1450 psi
@Temperature 1800 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.2 µm/m-°C
@Temperature 20.0 - 100 °C
6.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 13.4 W/m-K
@Temperature 20.0 - 100 °C
92.8 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 19.5 %19.5 %
Iron, Fe 4.0 %4.0 %
Nickel, Ni 75 %75 %
Titanium, Ti 0.40 %0.40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals NIMONIC® Alloy 75
Special Metals INCONEL® Alloy G-3
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
Haynes Hastelloy® S alloy, flat products
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 16000 hours

NZ97144 / 200206

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.